The Mini-Max pass-through parts washer features a 16-inch wide steel conveyor belt that carries the parts through a wash tunnel where parts are blasted with hot water spray from a 360-degree spray manifold. The conveyor belt, made of 1-by-1 inch flat wire mesh, can be adjusted to move at a speed of up to eight feet per minute. Parts are said to always be within 10 inches of the spray nozzles for cleaning impact. Water is heated by three nine-kw tubular heating elements to a temperature of up to 140°F. Models come in three different electrical configurations—230v, 460v and 575v, all three-phase—as well as a deluxe version with all wetted surfaces made of staingless steel. A five-hp vertical seal-less pump, with a high tolerance for metals and other solids in the wash water, delivers cleaning power of up to 110 gpm at 40-50 psi. Cuda also offers an entire line of detergents formulated to enhance the cleaning capability of aqueous parts washers.