This solution forms a high performance solgel hybrid coating after application to enhance the adhesion of paint systems.

Related Topics:

Socomore introduced Socogel, a blue acqueous surface pretreatment product made of zirconium salts that is activated by an organic-silicon compound. This solution forms a high performance solgel hybrid coating after application to enhance the adhesion of paint systems on metals, alloys and organic coatings. Socogel is a chromium-free conversion product that does not require rinsing after application. Socogel range products have been approved by several key aerospace manufacturers for preparation prior to painting or bonding and are used in many different industries