Specialty Plastics Filtration Systems Provide Corrosion Resistance

These systems have a standard filtration area of up to 430 ft2 and a filter gage of 0.2 to 100 microns.

�

Specialty Plastics Inc., Siebec filtration systems

 

Specialty Plastics Inc.’s Siebec filtration systems made with polypropylene (PP), polyvinylidene fluoride (PVDF) or stainless steel are designed for corrosion resistance on plating and industrial applications. These systems have a standard filtration area of up to 430 ft2 and a filter gage of 0.2 to 100 microns. With a maximum operating temperature up to 160°F (PP) or 230°F (PVDF), these filters can be used in a number of applications including electroplating baths, stripping baths, cleaning baths, degreasing baths and so on. 

 

For more information, visit spfinc.com.