Henkel Corp. has reformulated and reintroduced its Loctite 243 Threadlocker to withstand temperatures up to 360°F, cure consistently without primers, and tolerate contamination from thread lubrication, anti-corrosion and protection fluids. Designed for locking and sealing fasteners that may need to be disassembled during their service life, this anaerobic threadlocker now provides enhanced performance on both active and passive metal surfaces including steel, stainless steel, and plated materials, according to the company. Loctite 243 is available in 0.5 ml capsules, 10 ml tubes, and 50 ml, 250 ml or 1 liter bottles.