Vogel Industrial Coatings, the maker of high performance industrial coatings, reveals the T90, a reduced temperature cure and super durable TGIC Polyester powder coating.

Related Topics:

Vogel Industrial Coatings, the maker of high performance industrial coatings, reveals the T90, a reduced temperature cure and super durable TGIC Polyester powder coating. Peridium’s TGIC Polyester powder coatings feature tightly controlled particle size distribution that provides extremely good first pass transfer efficiencies. The T90 system can be cured at temperatures less than 300°F, and offers a wide cure window, ideal for parts with different metal thicknesses. These coatings typically provide long term exterior durability, are non-blooming, and have good over-bake resistance.