A new line of injection-molded vinyl tapered and threaded plugs combine the detailed design of injection-molded plastic and the soft pliable nature of vinyl, acordin gto developer Caplugs. The HETV series consists of heat-resistant, externally threaded plugs that can be easily pushed into place and have a pull-tab for easy removal. They are available in seven sizes, and teh viney’s flexibility enables them to fit a variety of port sizes. Manufactured from the company’s Flex500PLUS material that’s heat-resistant to 500ºF and beyond, the plugs are ideal for masking in powder coating, plating and other applications.