Translucent Powder Coatings from IFS Coatings

IFS Coatings exhibits a working powder booth and oven demonstrating translucent powder coating.

Related Topics:

IFS Coatings exhibits a working powder booth and oven demonstrating translucent powder coating. Users can spray the IFS translucent powder of their choice onto an aluminum water bottle, preprinted with the company’s logos.  When the powder is first sprayed onto the bottle, the logos are completely covered. Then, as the powder cures in the oven, the bottle is coated with the logo clearly visible beneath. In addition to translucent powders IFS Coatings displays hundreds of RAL colors, anti-graffiti powder, anti-microbial powder and even clear powder coats.