Transmet Corp.’s ZA4 Zinc Alloy Shop Removes Flash from Light Metal Castings

The durability of the shot is said to result in two-thirds less dust from blasting operations.

Related Topics:

Transmet Corp.’s ZA4 zinc alloy shot is designed to outlast the standard zinc shot by 50 percent and zinc-cut wire by 300 percent. The durability of the shot is said to result in two-thirds less dust from blasting operations. ZA4 is a relatively soft shot engineered for removing flash from light metal castings without damaging or warping parts. Shorter blast cycle times have also been reported as a result of switching to ZA4. Transmet tests every lot of zinc shot before shipment to ensure durability and performance for customers.