The Elcometer 1615 Variable Impact Tester, an instrument designed for evaluating the resistance of a coating to impact, elongation, cracking or peeling provides the user with a simple base instrument and a choice of six test kits, each comprising of all the items required to test in accordance with specific standards.

The Elcometer 1615 Variable Impact Tester, an instrument designed for evaluating the resistance of a coating to impact, elongation, cracking or peeling provides the user with a simple base instrument and a choice of six test kits, each comprising of all the items required to test in accordance with specific standards. Key features include: a comprehensive range of test kits; a graduated tube with engraved markings; a stop collar with adjustable settings; an integrated bubble level ensuring that the tester is perpendicular; and an easy-fix sample clamp.


Learn More

Related Suppliers

Elcometer

Zones

Supplier Categories


Therma-Tron-X
Finishing Equipment
SIDSP
Finishing Solutions
Magic Rack
Col-Met

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved