The Thermadep one-step, water-based coating process for metal products is now being offered by Houghton International through a partnership with Egyptian Coating Co. The process is designed for metals that require short-term rust protection, coloring, protection for shipping, or extended storage. Thermadep protective coatings—available clear and in a variety of colors—are applied by dipping heated parts into a bath of low-VOC, water-based polymer solution.