You are viewing products related to: Chromic Acid Anodizing

PUBLISHED: 3/29/2017

Military-Grade Aluminum Conversion Coating Technology Introduced to HVAC Market

Metal Processing International (MPI) and Chemeon Surface Technology team up to bring a new thin-film conversion coating to the HVAC market.


PUBLISHED: 5/6/2011

Conversion Coating for Aluminum

Aluminescent is a REACH, RoHS, WEEE and ELV compliant and MIL-DTL-5541F approved conversion coating for aluminum that will be on display in the Luster-On booth.