Digital Mobile Metrology Device Captures 2D, 3D Surface Maps in Milliseconds
5/3/2023GelSight Max, a portable digital metrology device, enables users to take repeatable measurements of roughness values down to the submicron level.
IFS Coatings Renews Architectural Powder Coating EDPs
4/27/2023IFS Coatings has renewed environmental product declarations (EPDs) for its range of architectural-grade powder coatings.
Blast Nozzle Features Enhanced Noise Reduction
4/27/2023Kennametal adds noise-reducing Blast Ninja to portfolio of abrasive blast nozzles.
Brighton Science Unveils Cloud-based Surface Intelligence Platform
4/25/2023Next-generation solution uses data and analytics to prevent bonding and adhesion issues.
Aqueous Cleaning Handbook Receives Update
4/21/2023The Aqueous Cleaning Handbook, authored by several members of Alconox Inc., is now in its 5th edition.
Architectural Powder Coating Mimics Natural Stone
4/17/2023AkzoNobel offers new stone effect powder coating for North American market.
Breathable Epoxy Flooring System for Floors With Elevated Moisture, Salts
4/8/2023The Vent-E is a breathable epoxy system for floors with elevated moisture and salts, creating a new market for epoxy floors, according to Dur-A-Flex.
MicroCare Offers Alternatives to Discontinued Vapor Degreasing Fluids
3/31/2023MicroCare says it is equipped to handle customers affected by 3M's discontinuation of the Novec specialty fluids line with its own products.
Hollow Cone Liquid Nozzle Provides up to 250 PSI Operating Pressure
3/30/2023The 1/2 NPT HollowStream liquid nozzle from Exair performs a variety of applications across the industry with a hollow cone spray pattern.
CHEMEON eTCP Powder Qualifies for MIL-DTL-81706B / MIL-DTL 5541F
3/21/2023The DoD-qualified products list (QPL/QPD) now includes eTCP Powder for corrosion protection and improved adhesion.