NOx Scrubbing Technology Breakthrough
This paper presents research findings and practical results that address the treatment of the problematic greenhouse gases nitrogen oxides (NOx) and sulfur dioxide (SO2).
Article: External Published: 1/24/2014
The Tribology of Contact Finishes for Electronic Connectors Part I: Mechanisms of Friction and Wear
This paper is an expanded treatment of the first part of the William Blum Lecture presented at SUR/FIN 1988 in Los Angeles by Dr. Morton Antler, 1987 AESF Scientific Achievement Award recipient. The subjects covered include friction, mechanical wear...
Article: External Published: 1/7/2014
Evaluation of Atmospheric Corrosion on Electroplated Zinc and Zinc-Nickel Coatings by Electrical Resistance (ER) Monitoring
This paper is a peer-reviewed and edited version of a presentation delivered at NASF Sur/Fin 2013 in Rosemont, Ill., on June 12, 2013.
Article: External Published: 1/7/2014
Electrodeposition of Ni-Fe-Mo-W Alloys - Part 3
3rd Quarterly Report - AESF Research Project #R-117 This paper was submitted to NASF and the AESF Foundation Research Board in October 2013 as a 3rd-quarter report of AESF Research Project #R-117.
Article: External Published: 12/1/2013
Selective Brush Plating a Tin-Zinc Alloy for Sacrificial Corrosion Protection
A tin-zinc selective brush plated coating has been developed to provide sacrificial corrosion protection without the use of toxic chemicals.
Article: External Published: 12/1/2013
Alloy Plating by Heating Stacked Single Layers and the Possibility of its Application in the Future
This paper was presented at NASF SUR/FIN 2013 in Rosemont, Ill., on June 10, 2013.
Article: External Published: 11/1/2013
Electroplated Tin-Nickel Coatings as a Replacement for Nickel to Eliminate Nickel Dermatitis
This paper is a peer-reviewed and edited version of a paper delivered at NASF SUR/FIN 2013 in Rosemont, Ill., on June 12, 2013.
Article: External Published: 10/29/2013
Electrodeposition of Ni-Fe-Mo-W Alloys - Part 2
This paper was submitted to NASF and the AESF Foundation Research Board in July 2013 as a 2nd-quarter report of AESF Research Project #R-117.
Article: External Published: 10/10/2013
Considerations Regarding the Proper Loading of Vibratory Finishing Bowls for Optimal Quality, Performance and Throughput Efficiency
Available since the late 1950s, traditional vibratory bowl processing has advanced in recent years from being a generic deburring tool to being able to achieve high-quality, isotropic superfinishes on critical, dimensionally-challenged workpieces. T...
Article: External Published: 10/10/2013
Electrodeposition of Ni-Fe-Mo-W Alloys - Part 1
This paper was submitted to NASF and the AESF Foundation Research Board in April 2013 as a 1st-quarter report of AESF Research Project #R-117.
Article: External Published: 9/17/2013

« Prev | | Next »


Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2015

Subscribe | Advertise | Contact Us | All Rights Reserved