Taking the (Oxide) Edge Off
Metal fabricators that laser-cut with oxygen take steps to prepare parts better for powder coating.
Article Published: 3/1/2013
Microabrasive Precision Shot Peening
Precision shot peening brings an entirely new concept to the field of microabrasive blasting, and it is complementary to its larger cousin. Using glass bead media, several companies have been shot peening for years with microabrasive blasting techno...
Article Published: 2/1/2013
Grinding Out a Polished Finish
Enerquip installed a special two-head OD polisher built by Grinding and Polishing Machinery of Indianapolis, Ind., a specialist in designing and building industrial grinding and polishing machinery. It uses the stainless pipes for the sanitary-grade...
Article Published: 12/1/2012
Turbo-Charged Abrasive Machining Offers Uniformity, Consistency
Method can deburr, produce edge contour effects rapidly
Article Published: 6/1/2012
Drag Finishing of Delicate Parts
For complex parts with high surface finish specs, production deburring and surface prep can be done using the drag finishing process whereby the parts to be deburred and finished are mechanically dragged through the media while attached to fixtures—...
Article Published: 10/1/2011
Making the Grade With Mechanical Media
Understanding media grades is important to good mechanical finishes.
Article Published: 7/1/2011
Mass Finishing: What is it All About?
Mass finishing refers to any deburring, edge breaking, or surface conditioning process in which the workpieces, although confined in a chamber, are not fixtured.
Article Published: 2/21/2011
Better Peening Shouldn’t Be a Shot in the Dark
Almost any pilot will tell you that when it comes to airplane parts like wings or engine blades, failure is unacceptable. That’s why more aerospace companies have sought to reduce the possibility of metal fatigue in such critical parts, and why some...
Article Published: 12/1/2010
Improving Aerospace Engines with Advanced Materials
Advanced ceramics and high performance superalloys are playing an important role in improving aerospace engines as aerospace manufacturers look for high-temperature materials that increase performance, improve fuel efficiency and satisfy safety stan...
Article Published: 12/1/2010
Baking Soda Solves Coating Build-Up Problem
More than 1,700 carriers are cleaned quarterly without interrupting production...
Article Published: 6/1/1996

« Prev | | Next »


Loading the player ...
Schaffner Mfg. Co., Inc.

Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved