Anodizing: Current Density vs. Voltage
Can you detail the procedure for anodizing using the current density method? What are the quality advantages for us to completely change our processing technique?
Ask an Expert Published: 10/24/2012
Glue Adherence to Black Anodize
Question We’re having a problem with glue not adhering to anodized parts made from extruded 6063-T6 aluminum and finished with heavy etch and black anodize per MIL-A-8625, Type II, Class 1. The problem parts come in batches, something lik...
Ask an Expert Published: 11/1/2008
Problems with Black-Dyed Parts
Recently, we’ve had rejected parts because the black dye is coming off when the parts are wiped down with DI water.
Ask an Expert Published: 11/1/2008
Anodizing Fundamentals
Question: I have just started my enterprise and couldn’t find any information on anodizing using a high start-up amperage versus a more slow and even increase of amperage within the first seconds of having the load in the tank.
Ask an Expert Published: 8/1/2008

« Prev | | Next »


Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved