Process

Exploring the: Process Zone

89 Results for: Experts

Sort by:
Published: 7/1/2017

Cathode Materials and Cathode/Anode Ratios
Q. Can we use titanium as a cathode in our Type I, II and III anodizing tanks, and what are the guidelines for cathode to anode surface area ratios?

Published: 4/1/2017

How to Carefully Maintain Your Alkaline Etching Bath
Q. What should be the maximum aluminum content in an alkaline etching bath to avoid galvanized appearance (spangling) when preparing 6063 T6 extrusions for Type II anodizing?

Published: 2/1/2017

Differences in Masking and Plug Materials
Q. Can you explain the differences between masking caps and plugs?

Published: 1/1/2017

Water Quality in the Anodizing Process
Q. I would like to know more about the physical and chemical parameters that are used to evaluate the quality of water used in the anodizing process.

Published: 1/1/2017

Anodizing Clinic: Sealing with Distilled Water
Q. Can distilled water be substituted for deionized water? Our facility can create a distilled water heated bath fairly easily because we already produce distilled water for another process. A DI water bath would be much more expensive. 

Published: 12/28/2016

Anodizing Clinic: Painting Parts After Anodizing; Seal, or No Seal?
Q. In conversations with our anodizer on the best way to seal parts for adhesion prior to painting, he referred to a choice of either a final hot water immersion at around 120°F with no seal or a hot water seal at a much higher temperature. What is ...

Published: 12/1/2016

Anodizing Clinic: Measuring Color of Coatings with a Colorimeter
Q. Recently, a company asked us to match its samples so we could do work for them. According to our method, we matched the samples, but they were rejected when they were sent to the company. We were told the samples were out of tolerance. We discove...

Published: 12/1/2016

Anodizing Clinic: Anodic Coating Blistering on 7075 Alloy
Q. We have recently run into a surface condition when hard anodizing 7075 machined forgings. It seems to be present primarily on the end of the part, even down into the hole. Both of these areas are machined. The condition does not appear to be evid...

Published: 11/3/2016

Anodizing: Corrosion on Hardcoat Anodized 7000 Series Forging
Q. I sent you photos of two parts that are alloy 7050 forgings. On these parts there are spots that appeared as a result of Type III (hardcoat) anodizing that were not present before anodizing. They look like corrosion of some sort, but the corrosio...

Published: 9/1/2016

Plating Clinic: Adhesion of Brush Plated Deposits
Q. How well does a brush-plated deposit adhere to the base metal?