Black, Pitted Areas on Anodized Parts
We anodize aluminum cookware and have recently been getting parts with black pits scattered all over them. What is this and how might it be happening?
Ask an Expert Published: 5/6/2013
Pink Coating on BSA Parts
I understand that iron and poor current can cause a pink coating on boric-sulfuric anodized (BSA) parts. What levels of iron are permissible before reaching the pink-colored coating? Are there any other things we could be missing?
Ask an Expert Published: 2/7/2013
Chemical Film Staining
What technique is used to avoid staining on aluminum parts when chemical film per Mil-C-5541 is applied?
Ask an Expert Published: 2/1/2013
Parts Burning During Hard Anodizing
What could cause parts to burn during hard anodizing?
Ask an Expert Published: 11/7/2012
Color Matching
We have an accepted color that we are using for a dyed anodized finish on 6061. Over the years, the approved color somehow went from an original production run coupon to a standard Pantone color. Unfortunately, the Pantone color doesn’t match the ap...
Ask an Expert Published: 8/3/2012
Hardcoat Anodize Thickness Problem
During the anodizing cycle, how can we check to see if the coating thickness is reaching the thickness requirement stated on the drawing?
Ask an Expert Published: 2/1/2012
Is it Anodized or Not?
What would be the best way to indicate whether or not an aluminum part has been electro-polished and anodized?
Ask an Expert Published: 2/1/2012
Technical References for Anodizing
Are there any resources to read and keep on hand as references for troubleshooting appearance issues?
Ask an Expert Published: 2/1/2012
Glue Adherence to Black Anodize
Question We’re having a problem with glue not adhering to anodized parts made from extruded 6063-T6 aluminum and finished with heavy etch and black anodize per MIL-A-8625, Type II, Class 1. The problem parts come in batches, something lik...
Ask an Expert Published: 11/1/2008
Hardness of Hardcoat Anodize
Question: What would be the hardness of the Alcoa Alumilite 226 hardcoat finish? The substrate is 6061 alloy aluminum tubing. G.S.
Ask an Expert Published: 11/1/2008

« Prev | | Next »


Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved