We have an aluminum casting from which we need to remove powder coat. We have investigated sanding and chemical, but the heat process may have a very negative impact on the part shape. What are your thoughts? Ask an ExpertPublished: 8/1/2010
We’re looking to install an in-line (or off-line) cleaning system that would degrease flat expanded metal sheet made out of 0.015-inch-thick SS T409 material. Ask an ExpertPublished: 4/1/2010
Our chemical supplier is telling us that variations in steel from different mills can produce huge differences in salt-spray results even though it is all cold rolled commercial quality steel. How much truth is there to this, and is there anything s... Ask an ExpertPublished: 2/1/2010
What effect, if any, will raising the temperature of RO water in a post-anodize, post-chromate rinse tank from ambient to 130°F have on the water’s pH value? Is there a way to rinse in hot RO water, max 130°F, and still be able to maintain a pH lev... Ask an ExpertPublished: 12/1/2007
I very rarely get a grease-like substance clinging to the surfaces of parts after I remove them from the pickling bath. Ask an ExpertPublished: 10/1/2007