Published: 12/1/2016

Anodizing Helps Yo-Yos Make a Colorful Comeback
One Drop Yo-Yos in Eugene, Oregon, is a leading high-end yo-yo manufacturer. It gets some of the 8,000 products it makes finished at Gruntbull Anodizing in Gettysburg, Ohio, whose splash anodizing process combines as many as six colors on the same p...

Published: 10/1/2016

Anodized Metal Maiden
Minnesota woman opens Premier Anodizing to complement her existing chain maille business and hoped to increase production of jump rings for jewelry to 1,000 a week. Now the business produces over a million a day.

Published: 6/1/2016

Aluminum Anodizer Implements Zero Liquid Discharge
Success of water minimization reuse at Bonnell Aluminum in Georgia after implementing zero liquid discharge facility for aluminum anodizers.

Published: 6/1/2016

Why Does Anodize Fade?
There are several causes not related to shops cutting corners and a specification should not be an excuse.

Published: 12/1/2015

Wreaking Havoc: Motorcycles Manufacturer Offers Online Coating Customization
Canadian firm starts custom design program.

Published: 6/1/2015

120 Years of the “Wolkerstorfer Way”
Minnesota finisher still growing after more than a century. Watch the VIDEO of the company.

Published: 11/1/2014

The Toughest Plater in America
SEE THE VIDEO: KMG Metal Finishing’s Kim Bossley is a plater, and a survivor after losing her shop and suffering through an often-fatal illness.

Published: 11/1/2014

Funky Medina Plating and Powder Shop
Owners Shawn Ritchie and Tait Krejci take an unorthodox approach to success.

Published: 9/1/2014

Science of Successfully Anodizing Die Cast Substrate
Die castings pose some of the most challenging problems in anodizing. This paper provides some explanations by tying together metallurgical science with anodizing practice.

Published: 12/1/2013

Anodizing that Withstands H2O2 Cleaning
Testing color anodized finishes in hydrogen peroxide gas plasma sterilization.