Published: 3/1/2017

How to Identify and Control Poor Ecoat Film Appearance
Q. We are experiencing textured ecoat on galvanized service parts and were told the galvanized coating is electrolytically applied with 60/60 zinc weights.

Published: 12/1/2016

Ecoat Clinic: High Throwpower Impacts Ecoat Performance
Q. Why is high throwpower so important to the overall applied cost for an electrocoat system? What specific elements of the system are affected by it? How can I measure the throwpower effect?

Published: 8/23/2016

Ecoat Clinic: Topcoat to Increase UV Protection
Q. We are using a cathodic epoxy electrocoat to prime our steel parts. Now our customer is asking us to start using an additional topcoat to increase UV protection from the sun. What paints are the best topcoats for cathodic epoxy electrocoats? Are ...

Published: 8/23/2016

Ecoat Clinic: Using Epoxy Ecoat on NdFeB Parts
Q. Is it possible to use an epoxy electrocoat to coat parts made out of neodymium, iron and boron? Are there any special considerations to take when electrocoating this kind of substrate?

Published: 6/1/2016

Electrocoating Q&A: Obtaining Class A Automotive Part Quality
We are upgrading our line to satisfy a new customer and want to make sure we cover all necessary upgrades.

Published: 3/1/2016

Electrocoating Q&A: Orange Peel Effects on Steel Parts
We are experiencing intermittent orange peel effects on steel parts that are zinc plated before phosphate and black epoxy ecoat paint.

Published: 3/1/2016

Electrocoating Q&A: Film Thickness Options
What type of epoxy ecoat do most automotive companies use for their steel parts?

Published: 12/1/2015

Electrocoat Q&A: Best Testing Practices
What are the best practices for testing an automotive electrocoat system?

Published: 9/1/2015

Electrocoating Q&A: The Challenge of Zinc-Coated Steels
What are the differences in adhesion performance?