What should be the expected transfer efficiency of a square transfer system composed of one e-coat bath and two permeate immersion tanks? Ask an ExpertPublished: 2/19/2013
What are the film thickness capabilities for an electrocoat? What are the maximum and minimum film thicknesses a system can obtain? What bath parameters can change the quantity of film deposited? Ask an ExpertPublished: 6/5/2012
Can electrocoat be used to coat copper and magnesium substrates? Do you know of any commercial applications using those metals? Ask an ExpertPublished: 2/27/2012
We are a plating company about to embark on the world of e-coat and are having a hard time deciding which type of machine to buy. Ask an ExpertPublished: 5/24/2011
We are facing lowering the CO2 emissions from our factory. Our biggest emission point is our electrocoat system. What areas can we change or better, to meet the stringent limits we have on our emissions? Ask an ExpertPublished: 1/11/2011
We are facing a problem of bad marks on our final e-coated automotive parts, which are most probably caused by dripping ultra filtrate. Ask an ExpertPublished: 6/1/2010
After 500 hours of salt spray SS testing of our electrocoated parts, we see many blisters but little corrosion increase from the test X-Cut. Ask an ExpertPublished: 6/1/2010
At the end of the process, when the body gets out of the E-coat bath, sometimes incomplete draining of the body can occur and this can produce problems during the baking phase. Could you tell me more about the nature of these problems? Do some speci... Ask an ExpertPublished: 12/1/2009