Black Stains After Curing
We are doing e-coating for small components like nuts and bolts, but are seeing black stains on the parts after curing.
Ask an Expert Published: 5/24/2011
E-Coat Stains
We are facing a problem of bad marks on our final e-coated automotive parts, which are most probably caused by dripping ultra filtrate.
Ask an Expert Published: 6/1/2010
Corrosion Blisters
After 500 hours of salt spray SS testing of our electrocoated parts, we see many blisters but little corrosion increase from the test X-Cut.
Ask an Expert Published: 6/1/2010
E-coat Pretreat
I’m looking for an environmentally friendly pretreat for reinforcing rods that are to be epoxy coated on a conveyor line. What is available in the market that can increase my cathodic E-coat performance?
Ask an Expert Published: 4/1/2010
Heat-treated Parts and E-coat
Heat treated parts paint a little differently than plain steel parts, so I will try to explain the differences.
Ask an Expert Published: 12/1/2009
E-Coat Prep
Question: Please advise if you know of a best practice for cleaning or other surface preparation for e-coating that needs to be “secondary crimped.” L.N.
Ask an Expert Published: 10/1/2004

« Prev | | Next »


Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved