Your frequent reference to the tri-cyl shape as being one of the most universal has been true for many jobs, but this is apparently an exception. Ask an ExpertPublished: 4/1/2009
When our mass finishing equipment is started after being shut down a week or more, an extreme stench emanates from the entire system. Ask an ExpertPublished: 4/1/2009
Some of the internal deburring processes will work under one set of conditions but not another, and most processes either involve a substantial capital investment or very high costs by outside contractors. We often use brushing, either by hand or se... Ask an ExpertPublished: 1/1/2009
We have encountered corrosion problems over the past few months and have examined every procedure to try and fix the problem. What have we overlooked? Ask an ExpertPublished: 10/1/2008
I am in continuous disagreement with my vibratory finishing operator regarding the flow rate of compound solution going into our 10 ft3 bowl vibrator. Can you give me some guidelines and supporting arguments? Ask an ExpertPublished: 7/1/2008
We have two problems: First, there is some nicking on the parts, and we have always wanted to reduce that effect; second, we are not satisfied with the production rate of 40 parts/hr per machine. Any suggestions? Ask an ExpertPublished: 4/1/2008
I recently viewed a custom motorcycle with highly polished stainless steel parts, including the large exhaust pieces.
The owner said the parts were tumbled. I examined the parts for the telltale surface marks of mass finishing, but I could see not... Ask an ExpertPublished: 4/1/2008