We test the adhesion of plastisol to steel by crosshatch cutting through the plastisol and galvanizing all the way to the steel substrate. Is this test reliable for paint film adhesion? Ask an ExpertPublished: 5/15/2013
Our stripping process sometimes does not remove all of the nickel plate. When re-plated, the areas that still have “old” nickel on the surface tend to flake. Do you have any suggestions for solving this problem? Ask an ExpertPublished: 5/10/2013
We plate carbon steel with brass, and our process consists of hydrochloric acid pickling, rinse, cyanide brass plating, or copper and zinc followed by diffusion. Would it be possible to plate stainless steel with the same process? Ask an ExpertPublished: 5/9/2013
Can you recommend a reliable company that can supply the equipment and install a line that would be able to paint corrugated tank radiators? Ask an ExpertPublished: 5/8/2013
Is there a process or commercial equipment to electrodeposit Zn, Ni, Cr, Fe, and remove the heavy metals from the wastewater? Ask an ExpertPublished: 5/7/2013
We anodize aluminum cookware and have recently been getting parts with black pits scattered all over them. What is this and how might it be happening? Ask an ExpertPublished: 5/6/2013