In the April issue there was a question about black paint having poor adhesion. You wrote about the oil absorption and bulking values of different pigments. I would have been interested in the gloss of his black paint. Ask an ExpertPublished: 9/1/2010
One of our customers has 48 steel valves ranging from from 6–48 inches. These valves were supplied to our customer coated with a high temperature one-pack silicone coating system. We have been instructed to repaint these valves. Ask an ExpertPublished: 9/1/2010
The same paint does not produce the same wrinkle texture when applied by the vendors—and we have tried different vendors. The only difference I can see is that we use electrically-fired ovens and they use gas-fired ovens. What do you think about thi... Ask an ExpertPublished: 9/1/2010
I am interested in coating PVC foam boards with paint. I heard that vacuum coating is a process that will work for this application. Can you direct me to a company that can either supply the equipment to vacuum coat, or provide the service to vacuum... Ask an ExpertPublished: 5/1/2009
We want to coat our wire (0.80 mm diameter) with a high viscosity UV ink as a thin layer (~20 µm). You have suggested in your article to use a 'wire tower.' Are there sample drawings or pictures of this system? Currently our line is running on a hor... Ask an ExpertPublished: 5/1/2009
I have built a log splitter from carbon steel. What is the easiest way for me to prepare the steel for painting with zinc oxide primer and implement paint? Ask an ExpertPublished: 5/1/2009
In this application the paint must last for several years in service without peeling, flaking or other deterioration. We have been getting customer complaints about paint peeling and flaking off the assemblies. What is the best way to solve our prob... Ask an ExpertPublished: 5/1/2009
I am an automotive paint formulator in the Middle East. Two weeks ago, our weather was rainy and we saw water spot defects on the horizontal surfaces of test specimens on our outdoor exposure racks. This was after the top coat curing step. We believ... Ask an ExpertPublished: 4/1/2009
We currently use an aqueous cleaning system for our chrome plated parts before wet coat mask painting. The system is designed for exterior automotive adhesion specs. Can a modern vapor degreasing system provide the same adhesion? Ask an ExpertPublished: 4/1/2009
Is there an industry standard for industrial equipment primer and paint Dry Film Thickness (DFT)? It seems like I have seen 3–5 mil thickness for both primer and paint for a total DFT of 6–10 mils. Ask an ExpertPublished: 4/1/2009