One reader has something to add about paint temperature to Carl's response in the December 2012 column regarding spraying high-viscosity paints. Ask an ExpertPublished: 2/28/2013
We are located in southern India, where the normal temperature is 30-40°C. How can we control the humidity and temperature in our spray paint booth? Ask an ExpertPublished: 10/2/2012
My group has responsibility for process specification BAC5736 regarding mixing of an epoxy primer. Here is my interpretation of the specification. Ask an ExpertPublished: 7/30/2012
We produce industrial storage cabinets and would like to change the manufacturing process sequence to paint the parts before welding them together. Ask an ExpertPublished: 7/10/2012
I am the machine shop supervisor for a company that makes indoor exercising equipment. Some of the component parts are electroplated while others are painted. We buy these parts already painted since we have no painting equipment in our shop at this... Ask an ExpertPublished: 2/27/2012
Q. I am a manufacturing engineer in a plant that produces small appliances. We are having trouble with a baking enamel. When a part is rejected because of a paint defect, we try to recoat it, but the second coat won’t adhere to the first, causing us... Ask an ExpertPublished: 12/14/2011
We are an American corporation with operations in India. For one of our applications, we use an epoxy primer (BMS 10-11Y, type I, class A, grade E, water-reducible epoxy primer, green 44-GN-011). Can you please clarify if our product is suitable for... Ask an ExpertPublished: 11/23/2011