We test the adhesion of plastisol to steel by crosshatch cutting through the plastisol and galvanizing all the way to the steel substrate. Is this test reliable for paint film adhesion? Ask an ExpertPublished: 5/15/2013
Should two-part epoxy paint be able to withstand a temperature of 450ºF for 3 1/2 min, which is required by the adhesive? What could be causing spotty adhesion failures demonstrated by the paint flaking off? Ask an ExpertPublished: 2/5/2013
Why will the film thickness gage read the coating thickness on the weld joints between two stainless steel pipes and on the flanges but not on the pipe itself? Ask an ExpertPublished: 1/4/2013
We have problems getting a consistently even distribution of a high-viscosity paint in the spray pattern, resulting in striping on the sprayed parts. To get better results, we are currently adding reducing solvents to lower the paint’s viscosity for... Ask an ExpertPublished: 12/4/2012
How can we cut phosphating dust after zinc phosphate and passivating stages, and reduce overspray losses in our water wash spray booth? Ask an ExpertPublished: 10/29/2012
We occasionally have problems with insufficient paint adhesion. Where would I find a lab to perform an in-depth analysis of the adhesion among the interface of our paint, a base coat and primer material? Ask an ExpertPublished: 10/26/2012
We are located in southern India, where the normal temperature is 30-40°C. How can we control the humidity and temperature in our spray paint booth? Ask an ExpertPublished: 10/2/2012