We have been experiencing white corrosion (zinc oxide) while our steel components are in storage. All of these assemblies are nitrogen-brazed components and then are subject to clear zinc plating.What do you think is the root of our problems? Ask an ExpertPublished: 5/22/2013
Do the AAMA powder coat specifications for extruded aluminum—AAMA 2603, AAMA 2604 and AAMA 2605—correlate to the application of steel materials? Ask an ExpertPublished: 5/22/2013
We test the adhesion of plastisol to steel by crosshatch cutting through the plastisol and galvanizing all the way to the steel substrate. Is this test reliable for paint film adhesion? Ask an ExpertPublished: 5/15/2013
Our stripping process sometimes does not remove all of the nickel plate. When re-plated, the areas that still have “old” nickel on the surface tend to flake. Do you have any suggestions for solving this problem? Ask an ExpertPublished: 5/10/2013