Painting Anodized Aluminum
Because of the changes in our factory manufacturing sequence and production line, we are storing these parts for at least 13 hours before they are painted. In a management meeting, we discussed whether the storage of these parts before painting, or ...
Ask an Expert Published: 1/10/2011
Paint Compatibility
One of our customers has 48 steel valves ranging from from 6–48 inches. These valves were supplied to our customer coated with a high temperature one-pack silicone coating system. We have been instructed to repaint these valves.