Humidity Levels for Powder Application
Could our problems with powder application be extremely low humidity levels during the winter?
Ask an Expert Published: 5/3/2013
“Water-Break-Free” Test
What is a “water-break failure” test?
Ask an Expert Published: 5/3/2013
Stripping Copper-Nickel-Chrome
Is there a method for stripping copper-nickel-chrome deposits from rejected zinc diecastings?
Ask an Expert Published: 5/2/2013
Water-Wash Spray in Cold Climates
Can we safely install a water curtain spray booth at a factory in Russia? Won’t the spray booth water start to freeze when the temperature reaches 0ºC? Is it not more advisable to install a dry filter booth in this climate?
Ask an Expert Published: 5/1/2013
Treating for BOD from E-Coat
What is the most effective treatment for reducing BOD anolyte? Is a small carbon absorption unit on the overflow line the solution?
Ask an Expert Published: 4/30/2013
Sealing Parts After Two Months
Is it possible and practical to seal hardcoat anodized (Type III) parts that have been in storage for about two months?
Ask an Expert Published: 4/29/2013
Reclaim in Batch Booth
Is equipment available for collecting and re-using powder from spray-to-waste, open-end-booth applications?
Ask an Expert Published: 4/25/2013
Stripping Tin from Copper
I recently received some old tin-plated copper to be replated. What methods can remove the old tin layer without harming the copper?
Ask an Expert Published: 4/24/2013
Pollution Control for Anodizing
What pollution control equipment do you recommend for a small aluminum anodizing operation with a 500-amp rectifier?
Ask an Expert Published: 4/23/2013
Anodize Cooling System Design
What material would you recommend for the chilling system that I need to install for my anodizing tank, which has a capacity of 1,800 L (475 gal)? Can I go for Type 316 stainless steel or copper pipe with lead plating?
Ask an Expert Published: 4/22/2013

« Prev | | Next »


Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved