Published: 7/1/2017

Turbine Repairs Call for Selective Brush Plating Solution
IPS uses in situ repairs to minimize downtime and maintain revenue flows.

Published: 7/1/2017

CAD Capabilities Bring Racking Solutions to Life
Production Plus uses AutoCAD from design to fabrication, streamlining production and ensuring maximum rack density.

Published: 7/1/2017

NASF Report: July 2017
NASF releases its Metals Loading Study for Wastewater Discharges and looks at recent federal deregulatory actions impacting surface finishing.

Published: 6/1/2017

Replacing Hex Chrome for Aerospace Applications
A collaboration develops between NASA and the European Space Agency to test and evaluate coating systems as replacements for hex chrome coatings in aerospace applications.

Published: 5/1/2017

Alkaline Zinc Systems Answer the Call for Integrated Solution
Asterion introduces a comprehensive plating system covering demands for productivity, corrosion resistance and appearance.

Published: 4/1/2017

Medina Plating Earns No. 1 Top Shops Status
Medina Plating’s operational performance earned it the distinction of being the No. 1 shop in the Products Finishing Top Shops Benchmarking Survey conducted in late 2016.

Published: 4/1/2017

Fixing Electroless Nickel Adhesion Issues
A shop plated a carburized AISI 8620 steel alloy with 15 microns of an 8-percent NiP electroless nickel deposit and acceptance by its customer. Now, the OEM requires that the shop switch to an EN deposit in the range of 5 percent. Coventya's Brad Du...

Published: 4/1/2017

Hohman Plating Practices Are Astronomical
Hohman Plating holds a client roll not for the weak of heart, which is why it has been named a Products Finishing Top Shop again in 2017 and earned honors for its Practices and Performance over the past year.

Published: 4/1/2017

2017 Top Shops Benchmarking Survey: Investments, Profits Are Trending Up
Analysis: Trends show more consistencies than differences over time; shops are increasing capital expenditures each year, with shops ranking at the top spending at 10 percent of gross sales.

Published: 3/1/2017

Surface Finishing Mexico Holds Second Show
Mexican Association for Surface Finishing expects 2,000 visitors.