Precision shot peening brings an entirely new concept to the field of microabrasive blasting, and it is complementary to its larger cousin. Using glass bead media, several companies have been shot peening for years with microabrasive blasting techno... ArticlePublished: 2/1/2013
Enerquip installed a special two-head OD polisher built by Grinding and Polishing Machinery of Indianapolis, Ind., a specialist in designing and building industrial grinding and polishing machinery. It uses the stainless pipes for the sanitary-grade... ArticlePublished: 12/1/2012
The correct peripheral speed is an important consideration in getting the right results from your buffing operation. A buff that is turning too fast or too slow may result in damage to the buff or to the workpiece. ArticlePublished: 1/1/2012
For complex parts with high surface finish specs, production deburring and surface prep can be done using the drag finishing process whereby the parts to be deburred and finished are mechanically dragged through the media while attached to fixtures—... ArticlePublished: 10/1/2011
When choosing vibratory media, understand the size, shape, starting roughness condition and metallurgical structure of the part. ArticlePublished: 7/13/2011
For fabricators, the finishing line is just the beginning of a new era in today's market. The days of simply cutting, bending and welding metal components into assemblies and delivering them to a customer in two to three weeks just don't exist anymo... ArticlePublished: 3/1/2011