We have had problems lately with light coating on our automotive products. We have started to clean the racks more often, and this seems to help a little, but we still are not getting the kind of coverage we got when the system was new. Ask an ExpertPublished: 2/21/2013
We use manual spray guns to apply a textured powder over a cast part, and that black finishes have a dark/light, splotchy look to them after they are cured.How can wer get better appearance? Ask an ExpertPublished: 2/19/2013
We have been using liquid paint for our architectural aluminum extrusions for about 20 years, but have considered using powder coatings to reduce our VOC and save cost. Can powder coatings meet AAMA 2604 and 2605 standards? What are the strengths an... Ask an ExpertPublished: 8/2/2012
Our powder booth takes about 30 min to change from one reclaim color to another. We are thinking of making a change, but I wondered how much production time we could gain if we invest in new equipment. What are my options, and how fast can you chang... Ask an ExpertPublished: 1/20/2012
We have been reviewing the costs of operating for our powder coating line and notice that gas is a big part of it. We have two heated stages in our washer, a dry-off oven, a cure oven and a burn-off oven. Can you give us any advice on ways to cut ou... Ask an ExpertPublished: 10/25/2011
We do recover some powder, and other colors are low volume, so we do not bother to recover them for reuse. But we are still throwing away a lot of material every year. Any suggestions on how we can get more value out of our powder? Ask an ExpertPublished: 9/23/2011
For several years we have operated our powder system without a room to enclose the booths and application process. It has worked out OK, but we need to make some adjustment for different humidity conditions. Is the cost of adding the room is justifi... Ask an ExpertPublished: 8/26/2011