Adhesion Failure on Galvanized Steel
We are having a big problem with powder coating on galvanized steel sheets.
Ask an Expert Published: 4/5/2011
Painting Anodized Aluminum
Can you tell me the pros and cons of painting anodized aluminum?
Ask an Expert Published: 3/31/2011
Powder Coating Hot-Dipped Galvanize
Do you know the procedure for powder coating galvanized steel?
Ask an Expert Published: 2/18/2011
Adhesion on Galvanized Steel
We just took on a new job for some parts that are hot-dipped galvanized and we are having big problems with adhesion failure.
Ask an Expert Published: 1/11/2011
Uniform Film Build
We cannot get uniform and consistent powder coverage up inside that two-inch deep channel.
Ask an Expert Published: 1/11/2011
Powder Coating Aluminum Extrusions
1) We have been told by some of our customers that they can buy powder coated products at cheaper prices than our liquid painted products. How do powder coaters paint for less than liquid paint? Is it labor, better transfer efficiency? What? 2) Whic...
Ask an Expert Published: 1/11/2011
Is Aluminum Harder to Paint?
How can I check to make sure we have a quality ground? Can I improve our ground, and how? Are there other things that we should do to improve our TE?
Ask an Expert Published: 1/11/2011
Adhesion Failure on Aluminum
We powder coat aluminum bench seats in 6061 and 6063 alloy and structural steel parts on the same line. We have had trouble with periodic adhesion failure on the aluminum parts.
Ask an Expert Published: 1/10/2011

« Prev | | Next »


Suppliers | Products | Experts | News | Articles | Calendar | Process Zones

The Voice of the Finishing Industry Since 1936 Copyright © Gardner Business Media, Inc. 2013

Subscribe | Advertise | Contact Us | All Rights Reserved