This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2012 in Las Vegas, Nev., on June 12, 2012. Article: ExternalPublished: 1/21/2013
This paper discusses a new advanced problem solving anodize technology for processing Types I, II and III anodize (A123) in a universal mixed electrolyte. This new chromium-free formulation will activate pore structure development, producing excelle... Article: ExternalPublished: 6/1/2012
When nickel electroplate is coupled with chromium, a high current density and corrosion rate at the anode, usually nickel, are favored by a high electrolyte concentration, a high temperature and a low nickel-to-chromium area ratio. Article: ExternalPublished: 4/1/2012
In the CASS testing of 1961 outside door handles plated in one of six exterior die-cast plating machines equipped for the dual chromium system at the Flint, Michigan plant of the Ternstedt Division of General Motors Corporation, 97% of the handles t... Article: ExternalPublished: 4/1/2012
In this work, well-aligned zinc oxide (ZnO) nanorods were successfully deposited on flexible polydimethyl-siloxane (PDMS) substrates by a simple hydrothermal growth method. The low temperature (<100°C) synthesized ZnO nanorods were investigated by s... Article: ExternalPublished: 2/15/2012
The stripping of electrodeposited and flame-sprayed coatings is a necessary part of surface finishing. Stripping may be required to allow for the re-plating of a part rejected due to defective finishing or as part of rework processes such as those c... Article: ExternalPublished: 2/15/2012
Electroless deposition of Ni-P-Al2O3 and Ni-P-TiO2, in the presence of gluconate as a complexing agent, on copper substrates was studied. The dependence of the composite formation on different plating variables was investigated. The deposited coatin... Article: ExternalPublished: 2/15/2012