Solving Wide-Body E-Coat Immersion Problems
4/1/2012
Products Finishing
-
Altec Industries in Burnsville, N.C., a manufacturer of heavy truck bodies and related equipment, added e-coat to its finishing operation and—through the proper design and execution of an electrocoat/liquid spray topcoat paint system —addressed issues of e-coating large truck bodies.
-
Measuring E-Coat Cure
2/28/2012
Products Finishing
-
What are the different ways to measure electrocoat cure? We use solvent rubs but, depending on the solvent, we obtain better or worse results of cure. How do we interpret this and what other tests can we do?
-
A “Bizarre” Approach: Using Moisture to Cure CARC Coatings
2/1/2012
Products Finishing
-
When veteran inventors Mike Bunnell and Daryl Bruischat put their minds together to build a better mousetrap for the drying and curing of waterborne CARC paints, they both hoped to come up with a system that might change the industry somewhat.
-
PF Expert: Electrocoating's Joe Tirado answers your questions
12/12/2011
Products Finishing
-
Have A Finishing Question? Joe tackles your questions in the E-coat Clinic.
-
Black Stains After Curing
5/24/2011
Products Finishing
-
We are doing e-coating for small components like nuts and bolts, but are seeing black stains on the parts after curing.