The Tribology of Contact Finishes for Electronic Connectors Part I: Mechanisms of Friction and Wear
This paper is an expanded treatment of the first part of the William Blum Lecture presented at SUR/FIN 1988 in Los Angeles by Dr. Morton Antler, 1987 AESF Scientific Achievement Award recipient. The subjects covered include friction, mechanical wear...

Published: 1/7/2014

Evaluation of Atmospheric Corrosion on Electroplated Zinc and Zinc-Nickel Coatings by Electrical Resistance (ER) Monitoring
This paper is a peer-reviewed and edited version of a presentation delivered at NASF Sur/Fin 2013 in Rosemont, Ill., on June 12, 2013.

Published: 12/1/2013

Electrodeposition of Ni-Fe-Mo-W Alloys - Part 3
3rd Quarterly Report - AESF Research Project #R-117 This paper was submitted to NASF and the AESF Foundation Research Board in October 2013 as a 3rd-quarter report of AESF Research Project #R-117.

Published: 11/1/2013

Alloy Plating by Heating Stacked Single Layers and the Possibility of its Application in the Future
This paper was presented at NASF SUR/FIN 2013 in Rosemont, Ill., on June 10, 2013.

Published: 10/29/2013

Electroplated Tin-Nickel Coatings as a Replacement for Nickel to Eliminate Nickel Dermatitis
This paper is a peer-reviewed and edited version of a paper delivered at NASF SUR/FIN 2013 in Rosemont, Ill., on June 12, 2013.

Published: 10/10/2013

Electrodeposition of Ni-Fe-Mo-W Alloys - Part 2
This paper was submitted to NASF and the AESF Foundation Research Board in July 2013 as a 2nd-quarter report of AESF Research Project #R-117.

Published: 9/17/2013

Electrodeposition of Ni-Fe-Mo-W Alloys - Part 1
This paper was submitted to NASF and the AESF Foundation Research Board in April 2013 as a 1st-quarter report of AESF Research Project #R-117.

Published: 9/10/2013

Corrosion Resistance of High-Phosphorus Electroless Nickel with a Lower Coefficient of Friction, Nanoparticle Codeposition Electroless Nickel Layer
This paper is a peer-reviewed and edited version of a presentation delivered at NASF SUR/FIN 2013 in Rosemont, Ill., on June 11, 2013.

Published: 5/20/2013

White Bronze, Copper-Tin-Zinc Tri-metal: Expanding Applications and New Developments in a Changing Landscape
This paper deals with the renewed interest in applications for white bronze tri-metal (Cu-Sn-Zn alloy).

Published: 4/18/2013

Method for Comparison of Leveling in Decorative Acid Copper Plating
Presented here is a test mechanism used to compare and contrast systems for leveling in acid copper plating as well as additives within a system.