Development of Ni-Based High Wear Resistance Composite Coatings
Hard chromium replacements have been actively sought for decades. In this, the Final Report for the AESF Foundation’s first Research Project since the formation of the NASF, the authors present the results of their extensive research into novel pla...

Published: 8/18/2011

Investigation of Tin Whisker Formation
Immersion tin and lead-free hot air solder leveling (HASL) coatings based on SnCu or SnAgCu alloys are widely used as surface finish materials for printed circuit boards (PCB). These coatings prevent the underlying copper from corrosion and preserve...