| 1 MINUTE READ

Powder Coating Film Thickness Goggles

Queston: Is there a type of goggle that will help to see coverage of part in the booth?

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Queston:

Is there a type of goggle that will help to see coverage of part in the booth? The paint is an ivory color and it is difficult to see thickness inside the booth. G. W.

Answer:

I could have a lot of fun with this question. For instance, I could ask if you are the subject of a lot of “dumb blond” jokes? Possibly you want to buy the Brooklyn Bridge. Maybe you have heard of the famous “rose colored glasses” (or beer goggles for that matter) and thought they might work to judge film thickness, as well. However, I will just give you the short and truthful answer…No!!!