Question: Can I repair titanium anode baskets?

Question:

Can I repair titanium anode baskets? J.B.

Answer:

Yes, titanium anode baskets can be repaired but it is best left to the vendor who originally supplied you with the baskets. Titanium must be welded under special conditions and is not a “do-it-yourself project.”