| 1 MINUTE READ

Asterion Video Demonstrates Hull Cell Analysis

Video shows platers how to run a hull cell, which is a testing tool in which an electroplating solution is evaluated across the range of operating conditions.
#plating #masking #pollutioncontrol

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon
�

 

 

A newly-produced video from Asterion in Indianapolis, Indiana shows platers how to run a hull cell, which is a testing tool in which an electroplating solution is evaluated across the range of operating conditions.

 

The video shows that an evaluation of the deposit on the cathode across a range of current densities is useful in demonstrating the capabilities of a plating bath solution:

 

Here's the video:

 

 

 

Asterion is a leading manufacturer of specialty chemical finishing products for all aspects of the metal finishing industry from a wide variety of pretreatment, to powder coating to plating. From traditional chemistries to innovative pollution preventive technologies. Asterion finishes are utilized worldwide to produce products, including automobile components, consumer appliances, industrial tools, furnishings and countless other items.

 

For more information on Asterion, click HERE to visit their website and the HERE to see the transcript of the video.

RELATED CONTENT

  • Masking for Surface Finishing

    Masking is employed in most any metal finishing operation where only a specifically defined area of the surface of a part must be exposed to a process. Conversely, masking may be employed on a surface where treatment is either not required or must be avoided. This article covers the many aspects of masking for metal finishing, including applications, methods and the various types of masking employed.

  • Chromium Plating

    An overview of decorative and hard chromium electroplating processes.

  • Plating Q&A: Can you color stainless steel?

    Our expert, Art Kushner, says yes, you can color stainless steel, but it is not a process that is typically performed in a plating shop. Read more about his answer.