Dassault Aviation Qualifies PPG Ecoat Aerospace Primer


#masking #aerospace #pollutioncontrol

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon
p

 

 

PPG has qualified its proprietary Aerocron electrocoat aerospace primer at Dassault Aviation for application to structural aircraft parts for corrosion resistance. Qualification to DGT153703 enables Dassault subcontractors to produce parts for the aircraft manufacturer using the chrome-free PPG e-coat primer.

 

According to Daniel Bencun, PPG segment manager for aerospace coatings in the Europe, Middle East and Africa region, the Dassault qualification demonstrates growing interest in the advantages of PPG’s ecoat primer.

 

“Throughout its history, Dassault has been an innovator and aviation industry leader, and qualifying Aerocron primer shows Dassault’s continued commitment to technological advancements and the environment,” Bencun said. “In addition to its many application and performance benefits, Aerocron primer is chrome-free and water-based, and it reduces emissions as well as waste-treatment requirements.”

 

In the e-coat process, metal parts are immersed into the electrically charged Aerocron primer bath. Compared with traditional spray primer application, PPG’s e-coat process provides better corrosion protection, more uniform application, and less coating weight for cost savings and enhanced aircraft fuel economy. Product utilization with Aerocron primer is significantly higher with no overspray, eliminating related worker exposure and producing near-zero waste.

 

“Dassault aircraft operators will benefit from the reduced weight of coated parts and superior corrosion resistance with Aerocron primer,” Bencun said. “While it is difficult to spray on a primer with a consistent coating thickness, Aerocron primer achieves a uniform thickness even on hidden and recessed areas of a part, a significant advantage important within the aerospace industry. Weight savings can be about 30 percent for flat parts and up to 75 percent on complex-shaped parts.”

 

Aerocron primer is also qualified to SAE International’s Aerospace Material Specification 3144 for anodic electrodeposition primer for aircraft applications.

 

PPG’s global aerospace business offers coatings, sealants, transparencies, packaging and application systems, and transparent armor, as well as chemical management and other services. For more information, visit ppgaerospace.com.

RELATED CONTENT

  • Troubleshooting for Electrocoating

    Characterizing the type of defect is essential in identifying the root cause and eliminating its source...

  • Measuring the Surface Area of Fasteners

    How do you measure the surface area of a threaded fastener? How much coating would you put on it? How thick of a coating? What about non-threaded fasteners? The U.S. Department of Agriculture’s Forest Service, of all people, may have come up with the solution for those pondering how to coat sometimes-difficult small pieces using computer imaging and software to compute the area.

  • Waterborne painting process is a first at South Carolina BMW plant

    PPG launched the first use of waterborne compact paint technology in a U.S. automotive manufacturing plant at the BMW assembly plant in Spartanburg, S.C. This painting process has turned out to be a 2012 award winner and has opened up a new way for auto manufacturers to go leaner and become more efficient in their operations.