The approved zinc plating systems include the use of Technibrite AZ 130 alkaline, non-cyanide zinc or the ZN 200 chloride acid zinc, followed by Technicoat ZnBl 360 trivalent passivate.

Harley-Davidson has approved Asterion’s Technibrite alkaline and acid zinc plating systems for its motorcycle powertrain components, meeting the company’s zinc plate and seal per ESPEC 805-050, and its zinc plate per ESPEC 805-051 specification.

The approved zinc plating systems include the use of Technibrite AZ 130 alkaline, non-cyanide zinc or the ZN 200 chloride acid zinc, followed by Technicoat ZnBl 360 trivalent passivate. Techniguard F 108 sealant is used to meet the ESPEC150 specification for Harley-Davidson.

Blair Vandivier, president of Asterion, says his company worked with distributor Hydrite Chemical Company on the Harley-Davidson approval process, which imparts a silver-white (clear) finish.

Related Topics

RELATED CONTENT

  • Citric Acid Passivation of Stainless Steel

    An alternative product for passivation...

  • Coating Thickness Measurement: The Fundamentals

    A review of available test methods, common applications and innovative instrumentation...

  • Masking for Surface Finishing

    Masking is employed in most any metal finishing operation where only a specifically defined area of the surface of a part must be exposed to a process. Conversely, masking may be employed on a surface where treatment is either not required or must be avoided. This article covers the many aspects of masking for metal finishing, including applications, methods and the various types of masking employed.


Resources