Curtiss-Wright’s Surface Technologies Division (Parsippany, N.J.), a global provider of highly engineered surface treatments and analytical services, has announced that its proprietary Microseal impingement lubricant coating process has been used on numerous components for NASA’s Mars 2020 Mission, many within the Sample Caching System on the Perseverance Rover.
“High performance in harsh conditions typical to space applications demands a reliable solution like Microseal,” says David Rivellini, senior vice president and general manager, Curtiss-Wright Surface Technologies. “The Microseal process outperforms conventional lubricants as it remains stable under extreme conditions and is resilient to shock, radiation, vibration, acceleration and electrical discharge.”
Featured Content
According to Curtiss-Wright, the Microseal process results in an ultra-thin self-limiting and firmly adherent solid film that only fills voids on the surface. The film is designed to perform in hard vacuums and in extreme temperatures ranging from -423˚F to 2000˚F (-253˚C to 1093˚C). Static, sliding and rolling load-bearing modes are all compatible with the process and application will not affect the base material’s hardness, temper, flexibility or other properties.
The company says the process creates a continuous lubricating surface that reduces friction and prevents galling and seizing. It also dissipates heat, remains stable under extreme environmental conditions, and does not attract contaminant particles. The process can be adapted to a wide variety of substrates.
NASA’s Mars 2020 Mission is scheduled to launch on July 30, 2020 from Cape Canaveral Air Force Station, Florida. Perservance’s mission is to seek signs of past microbial life and collect rock and soil samples for potential return to Earth.
RELATED CONTENT
-
Phosphate Conversion Coatings
Types of phosphate conversion coatings, how to apply them, and their specific functions.
-
Understanding Paint Atomization
BASF coatings development expert Tim December explains how paint atomization works for both pneumatic spray applicators and high-speed rotary bell applicators.
-
Pretreatment for Painting
Better adhesion, enhanced corrosion and blister resistance, and reduced coating-part interactions make pretreatment a must.