What's the Best Coating Method for Extended Outdoor Performance?
For long-lasting powder coating that holds up outdoors, consultant Rodger Talbert suggests pretreatment and washing options, a primer layer and a top coat.
#ask the expert
Q: We are a manufacturer of indoor furniture and we are currently planning to add an outdoor line to our offerings. This will include cast iron, steel fabrications and aluminum chairs and tables. What is the best way to powder coat the metal furniture to achieve high performance and longevity from the coating?
A: Outdoor performance brings a variety of elements into play that break down a coating. Sun, wind, rain and temperature can take a toll on even the toughest coatings. Before you select a coating, you need to decide how high you want to reach. The levels of performance can range from modest expectations to extremely high standards. As performance increases, so do process needs and cost.
Featured Content
Also, you need to know that outdoor performance is affected by the method used to prepare the metal and the metal substrate material as well as exactly how the product is manufactured. There are a lot of decisions to make so I will try to share some general guidelines to help you understand the options.
Pretreatment could be as simple as a cleaning and iron phosphate process. This will give you a good, clean surface and good powder adhesion to the substrate. It does not add any appreciable gain in corrosion resistance if the coating is damaged and moisture gets through to the substrate. To add corrosion resistance to the substrate, you will need to add a more robust conversion coating, such as zirconium oxide, zinc phosphate or chrome/non-chrome treatment. Zinc phosphate enhances steel substrates, but it also adds a lot of demands on the process side and complicates environmental responsibilities. Chrome is still used for aluminum, but it has been largely replaced by high-performing zirconium products or non-chrome conversion coatings for aluminum. The decision on what to use relates to the substrates being coated and how reliant you want to be on the pretreatment for corrosion protection.
Another way to enhance corrosion protection is the use of a high-quality primer. Powder primer can contain zinc for added protection, but even a standard epoxy primer will elevate performance a lot. Zinc-containing primers work best on blasted steel because the zinc makes better contact with the steel and therefore provides better cathodic reaction for corrosion protection. For smooth surfaces that are not blasted, the zinc has less benefit.
A primer layer offers more benefits than may be obvious: it adds to thickness for better moisture resistance and mechanical performance, it rounds out the edges for better coverage and protection against corrosion in these critical areas and it helps to fill areas that might be missed with a single coat.
With your variety of substrates and desire for long finish life, you will need to consider some alternative options. For wrought iron and steel fabrication with welds, you should consider blasting. Use a pressure blast for manual preparation or, if the volume is high and you have the capital, an inline-wheel blast system. Avoid blasting with steel shot or grit as it can leave behind ferrous iron and cause rust. Use garnet, aluminum oxide or something else. Wheel-blast systems may limit your media options because the media is hard on the blast system, so an aggressive media may wear the equipment out too fast.
You should also consider a washer for cleaning and application of a conversion coating. Zirconium oxide or similar transitional metal processes should be a good selection for a wide variety of metals. Having the options to blast or wash will give you a good start on the process.
Install a booth and an oven for primer. The primer-coat is applied and gelled (partially cured) and then the topcoat is applied. The two coats are finally cured in a second oven.
The options I suggest are based on your desire to achieve a high-quality product. You can compromise if you choose to have different-quality offerings or think the cost will be too high for your market. But if you are looking for quality and flexibility, this is the best set of options
Rodger Talbert
Rodger Talbert began his career in coatings in 1976 when he went to work for a small company that does metal fabrication and custom coating. He worked there for 10 years, rising to the position of VP of Sales and Marketing. He left there to work as a sales engineer for a larger company that designs and builds coating systems, and worked there for seven years. In 1993, Talbert started his own business as a consultant. He ran his own corporation for 15 years before joining The Powder Coating Institute as technical director in 2009. He served as the PCI Executive Director until June 2012.
RELATED CONTENT
-
Developments and Trends in Powder Coating
New solutions for powder coating centers combine powder preparation, conveyance, dosing and color changes into a fully automated, closed system.
-
Improving Transfer Efficiencies in Coating Operations
There are many methods for addressing electrostatic grounding in metal painting processes, and Tim Ulshafer from Mueller Electric says the best method for your process is a simple and worthwhile exercise.
-
TGIC Powder Coatings vs. Non-TGIC Powder Coatings
As raw materials become increasingly scarce, powder coating consultant Rodger Talbert offers insights into using non-TGIC products.