The Chrysler Corp. has granted PS-508 specification approval to Coral Chemical Co.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

The Chrysler Corp. has granted PS-508 specification approval to Coral Chemical Co. The designation means Coral Chemical has met all of Chrysler’s system pretreatment requirements with its zinc phosphate and iron phosphate metal treatment systems. The company also offers a variety of metal cleaners and sealing rinses to compliment zinc and iron phosphate coatings and meet the PS-508A and PS-508B requirements of this specification.

For more information on Coral Chemical, please call 800-228-4646 or visit coral.com