The average liquid and powder coating shop has five lines in operation, according to the 2017 Products Finishing Top Shops Benchmarking Survey.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

The average liquid and powder coating shop has five lines in operation, according to the 2017 Products Finishing Top Shops Benchmarking Survey. The median is three lines per shop, while the Top Shops averaged six lines per operation. All other shops had about two lines in operation.