Exair's 1” High Power Stainless Steel Flat Super Air Nozzle produces a flat 1" (25-mm) wide airstream with a blowing force of 16 ounces (462 g) when mounted 12" (305 mm) from the target.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Exair's 1” High Power Stainless Steel Flat Super Air Nozzle produces a flat 1" (25-mm) wide airstream with a strong blowing force of 16 ounces (462 g) when mounted 12" (305 mm) from the target. The nozzle design is said to be an ideal fit for both tight spaces and tight budgets.  The Type 316 stainless steel construction is suitable for corrosive, high temperature, food, pharmaceutical and chemical environments.

The air nozzle maximizes entrained airflow while reducing noise levels. A precise amount of compressed air is released through the 0.025" (0.64mm) air gap opening that is set with a stainless steel shim positioned between the body and removable cap. The airstream pulls in surrounding room air to produce a forceful stream of high velocity, laminar airflow. Sound level is low at 82 dbA, and it is CE compliant.  Force and flow may be adjusted by installing different shim thicknesses. Optional swivel fittings and Stay Set Flexible Hoses to aim the nozzle are also available.

The air nozzle is also available in zinc aluminum alloy construction and is suitable for rugged industrial applications.

Applications include ejecting heavy parts and slugs, chip removal, part cleaning, drying, liquid blowoff and cooling.