Alkaline Detergent Designed for Difficult Cleaning Applications

Madison Chemical's Clean-Gard 83 suited for ultrasonic cleaning.
#plating

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

Madison Chemical’s Clean-Gard 83 is an alkaline detergent designed for removing aged, oxidized, burned-on oil and grease, and for other difficult cleaning operations. It is intended for immersion application, including ultrasonic and agi-lift, as well as recirculation spray washers up to 25 psi. According to the company, it cleans more thoroughly in less time, thus increasing productivity. It is said the formulation produces low-to-moderate foam, which helps maximize ultrasonic cavitation. The company says that when the cleaning solution is not rinsed, it offers rust protection. It was developed for use with ferrous, aluminum and zinc alloys.

Visit Madison Chemical.

 