Asterion’s Technicoat Passivate Produces Blue Finish

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon

This product is formulated to produce a consistently blue, bright finish when applied to electroplated zinc.

Share

Facebook Share Icon LinkedIn Share Icon Twitter Share Icon Share by EMail icon Print Icon
�

Asterion LLC, Technicoat ZNBL 360 Ultra

 

Asterion LLC’s Technicoat ZNBL 360 Ultra is a trivalent, high-corrosion, thin-film passivate designed for electrogalvanized zinc. This product is formulated to produce a consistently blue, bright finish when applied to electroplated zinc, or it can be used as trivalent yellow. The company says this passivate meets 192 hours of neutral salt spray to white corrosion products without a top coat or seal.